KJM26 Insulating Firebrick is engineered for high thermal stability, strength, and sustainability. Made from carefully selected magnesia raw materials, enhanced through patented modification technology, and combined with high-purity silica, it forms a stable magnesium silicate crystalline phase for superior performance.
Manufactured using an advanced dry pressing process and high-temperature firing in a tunnel kiln, KJM26 bricks ensures uniformity and high density without the need for post-production cutting or grinding. Made entirely from natural minerals, it eliminates burn-out materials, reduces dust emissions, and enhances worker safety, making it a cost-effective and eco-friendly insulation solution for high-temperature applications.
✅ Optimized Bulk Density (0.8 g/cm³) – Matches ASTM 26 while offering better insulation than ASTM 28.
✅ Superior Strength (3.3 MPa CCS) – Stronger than ASTM 26 (2.0 MPa) and ASTM 28 (2.8 MPa), ensuring durability.
✅ Minimal Shrinkage (+0.2% @ 1450°C × 12h) – Tiny linear shrinkage, reducing volume change risk.
✅ Higher RUL (1370°C) – Withstands more heat than ASTM 26 (1250°C) and ASTM 28 (1350°C).
With better performance, durability, and cost-efficiency, KJM26 is the ideal upgrade for high-temperature applications. 🚀
KJM26 Insulating Firebrick are versatile and ideal for hot face refractory lining or back-up insulation in various industries, including:
| KJM26 Brick vs Traditional ASTM /GB Standard Insulating Firebrick | ||||||
| ASTM C155 – 2018 & China GB/T 35845 – 2018 Standard | ||||||
| New Product | Traditional Insulating Firebrick | |||||
| Grade | Standard | Unit | KJM26 | ASTM26 | ASTM27 | ASTM28 |
| Classification Group | ISO 2245 | 145-0.8-L | 140-0.8-L | 145-0.8-L | 150-0.9-L | |
| ASTM C155 | 26 | 26 | 27 | 28 | ||
| Classification Temperature | ℃ | 1450 | 1400 | 1450 | 1540 | |
| Bulk Density | ASTM C134 | g/cm3 | 0.8 | 0.8 | 0.85 | 0.9 |
| Cold Crushing Strength | ASTM C133 | MPa | 3.3 | 2 | 2.5 | 2.8 |
| Modulus of Rupture | ASTM C133 | MPa | 1.8 | 1.4 | 1.5 | 1.5 |
| Permanent Linear Change @ ℃×12h |
% | 0.2 | -1.5~+0.5 | -1.5~+0.5 | -1.5~+0.5 | |
| 1450 | 1400 | 1450 | 1510 | |||
| 0.05MPa Refractoriness Under Load |
℃ | 1370 | 1250 | 1300 | 1350 | |
| Thermal conductivity | ||||||
| 400℃ | ASTM C182 | W/m.K | 0.26 | 0.23 | 0.3 | 0.3 |
| 600℃ | 0.29 | 0.27 | 0.32 | 0.32 | ||
| 800℃ | 0.34 | 0.3 | 0.35 | 0.35 | ||
| Chemical Composition | ||||||
| Al2O3 | % | 55 | 60 | 65 | ||
| SiO2 | 65 | 42 | 36 | 33 | ||
| Fe2O3 | 0.5 | 0.9 | 0.8 | 0.7 | ||
| MgO | 27 | |||||